Any (brand filament profile) / PETG / ASA (general by material type)

PETG / ASA (general by material type) on Any (brand filament profile)

guide
Test on scrap first. Settings are starting points from the linked source. Dry hygroscopic filaments before printing.
Printer
Any (brand filament profile)
Filament brand
Polymaker
Filament type
PETG / ASA (general by material type)
Slicer
OrcaSlicer / Bambu Studio / PrusaSlicer
Nozzle size
0.4 mm
Nozzle temp
PETG 220–260 °C (230–240 optimal); ASA 240–260 °C
Bed temp
PETG 65–90 °C; ASA 90–110 °C; PLA 50–60 °C
Chamber / enclosure
ASA: enclosure required
Speed
PETG ≤ 60 mm/s print, 120 mm/s travel
Retraction
PLA 1–2 mm direct drive / 2–5 mm Bowden @ 30–80 mm/s
Cooling
PLA 100% (off first 0.5 mm); PETG 30–50%; ASA 10–25%
Notes
Polymaker wiki printing tips by material type. PLA min layer time ≥3 s. Wait for textured PEI to cool fully before removing PET-GF/PET-CF parts. ASA supports: HIPS or breakaway, interface density 75–90%.
Source: Polymaker